Application Of 1700 degree Alumina Fiberboard

Mar 15, 2022

The alumina fiber board produced by polycrystalline alumina fiber cotton, inorganic refractory aggregate, powder, special additives and special production process. The main crystal phase is corundum phase and a small amount of mullite phase. The long-term service temperature is greater than 1650 degree , 1700 degree . The alumina fiber board has good high temperature stability, low thermal conductivity, low heat capacity, thermal shock resistance and corrosion resistance, It is resistant to flame and airflow erosion, easy to process, cut and install. The product specifications are 900 600 15-150mm, 1000 600 15 150mm. The products are widely used in the lining of high-temperature furnace with temperature resistance above 1650 degree , roller kiln, aluminum melting furnace and heat treatment furnace.